SONG Zuodong. Construction Control and Prevention of Cracks in the Base of CRTSⅢ Slab Ballastless Track[J]. Intelligent Building and Construction Machinery, 2022, 4(1): 52-54.
Citation: SONG Zuodong. Construction Control and Prevention of Cracks in the Base of CRTSⅢ Slab Ballastless Track[J]. Intelligent Building and Construction Machinery, 2022, 4(1): 52-54.

Construction Control and Prevention of Cracks in the Base of CRTSⅢ Slab Ballastless Track

  • Received Date: 2021-12-16
  • Rev Recd Date: 2021-01-20
  • Available Online: 2022-03-28
  • Publish Date: 2022-01-28
  • Based on the CRTS Ⅲ slab base concrete structure, combined with the characteristics of the cracks in the CRTS Ⅲ slab ballastless track base of the Jinan-Qingdao high-speed railway, this paper analyzes the 56d shrinkage rate of concrete and the influence of early hydration heat on the base concrete, and summarizes the influence of the cracks on the concrete base. From the aspects of concrete ratio, material selection, pouring time period, maintenance method comparison and selection, etc., optimized technological measures are taken to control the occurrence and development of cracks in the base of CRTS Ⅲ slab ballastless track.

     

  • loading
  • [1]
    李昌宁,戴宇.郑徐铁路客运专线CRTSⅢ型板式无砟轨道施工关键技术[J].铁道标准设计,2015(9):25-28.
    [2]
    铁建设【2010】241号.高速铁路轨道工程施工技术指南[S].
    [3]
    TB10424-2010.铁路混凝土工程施工质量验收标准[S].
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (132) PDF downloads(8) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return